Thermal Effects during Plastic Flow in Nickel-Base Superalloys

B. Lisieki, L.P. Kubin, Y. Estrin

    Research output: Contribution to journalArticle

    Original languageEnglish
    Pages (from-to)10-10
    JournalMetallurgical Science & Technology (Italy)
    Volume10
    Publication statusPublished - 1992

    Cite this

    @article{eb56758e62a74d30afb6fbfb345f5475,
    title = "Thermal Effects during Plastic Flow in Nickel-Base Superalloys",
    author = "B. Lisieki and L.P. Kubin and Y. Estrin",
    year = "1992",
    language = "English",
    volume = "10",
    pages = "10--10",
    journal = "Metallurgical Science & Technology (Italy)",
    issn = "0393-6074",

    }

    Thermal Effects during Plastic Flow in Nickel-Base Superalloys. / Lisieki, B.; Kubin, L.P.; Estrin, Y.

    In: Metallurgical Science & Technology (Italy), Vol. 10, 1992, p. 10-10.

    Research output: Contribution to journalArticle

    TY - JOUR

    T1 - Thermal Effects during Plastic Flow in Nickel-Base Superalloys

    AU - Lisieki, B.

    AU - Kubin, L.P.

    AU - Estrin, Y.

    PY - 1992

    Y1 - 1992

    M3 - Article

    VL - 10

    SP - 10

    EP - 10

    JO - Metallurgical Science & Technology (Italy)

    JF - Metallurgical Science & Technology (Italy)

    SN - 0393-6074

    ER -