Application of Atomic Hirshfeld Surface Analysis to Intermetallic Systems: Is Mn in Cubic CeMnNi4 a Thermoelectric Rattler atom?

  • M.R.V. Jorgensen
  • , I Skovsen
  • , H.F Clausen
  • , J.L Mi
  • , M Christensen
  • , E Nishibori
  • , Mark Spackman
  • , B.B Iversen

Research output: Contribution to journal › Article › peer-review

Original languageEnglish
Pages (from-to)1916-1924
JournalInorganic Chemistry
Volume51
DOIs
Publication statusPublished - 2012